Customization: | Available |
---|---|
Feature: | Oxidative Degradable |
CAS No.: | 9003-55-8 |
Still deciding? Get samples of $ !
Request Sample
|
Suppliers with verified business licenses
Audited by an independent third-party inspection agency
Techinica data sheet | Standard | Unit | Value |
Physical | |||
Density | ASTM D-2240 | g/cm3 | 1.19 |
Molding Shrinkage | ASTM D-2240 | % | 1.3 |
Melt flow rate | ASTM D-2240 | g/10min | 2-8 |
Mechanical | |||
Tensile Strengthat yeild | ASTM D-412 | MPa | 25-30 |
Tensile Strength100% strain | ASTM D-412 | MPa | 3.5±0.1 |
Tensile Strength300% strain | ASTM D-412 | MPa | 6.5±0.1 |
Tear Strength | ASTM D-624 | N/mm | 60-75 |
Elongation at break | ASTM D-412 | % | 500-700 |
Shore Hardness | ASTM D-2240 | A | 75±1 |
Abrasion Resistance | ISO 4649 | mm3 | 45-50 |
Thermal | |||
Brittleness temperature | ASTM D-2240 | ℃ | <-60 |
Compressive Set 70℃ 22h | ASTM D-395 | % | 47 |
Compressive Set 23℃ 24h | ASTM D-395 | % | 15 |